Haynes 25(UNS R30605)
|
Introduction Haynes 25 is a Co-Ni-Cr-W alloy that combines excellent high-temperature strength with good oxidation resistance. |
|
Characters HAYNES 25 is a cobalt-nickel-chromium-tungsten alloy that combines excellent high-temperature strength with good resistance to oxidizing environments up to 1800° F (980° C) for prolonged exposures, and excellent resistance to sulfidation. It can be fabricated and formed by conventional techniques, and has been used for cast components. Other attractive features include excellent resistance to metal galling. |
|
Application HAYNES 25 combines properties which make it suitable for a number of component applications in the aerospace industry, including parts in established military and commercial gas turbine engines. In modern engines, it has largely been replaced by newer materials such as HAYNES 188 alloy, and, most recently, Haynes 230 alloy, which possess improved properties. Another area of significant usage for Haynes 25 is as a bearing material, for both balls and races. |
|
Equal grades UNS R30605, L605, GH5605(China), Werkstoff 2.4964 |
|
Chemical composition(%) C 0.05-0.15 Ni 9.00-11.0 Fe 3.00 max Si 1.00 max Mn 1.00-2.00 P 0.03 max S 0.03 max Cr 19.0-21.0 Co Remainder W 14-16 |
|
Standard AMS 5537 (sheet, strip and plate), AMS 5759 (bar, rings and forgings), AMS 5796 (welding wire), AMS 5797 (coated welding electrodes). |
|
Forms of product available at A-one Alloy Plate, sheet, strip, bar, forging, ring |
|
Delivery Available on request |
*Haynes is a registered trademark of Haynes International, Inc.
About A-ONE Alloy
Suzhou A-one Special Alloy Co. Ltd- referred as A-ONE Alloy hereafter, is a professional manufacturer of high performance alloy products. A-ONE Alloy is engaged in supplying high quality and cost effective Superalloy, Anti-Corrosion Alloy, Precision Alloy, Special Stainless Steel and Magnetostrictive Material to customers from worldwide.
Why A-ONE Alloy
· Rich experience in alloy industry
· Top rank experts of industry in China
· Advanced technology and process from top famous institutes in China
· Advanced devices through whole production and inspection process
· Strict quality control system
· Company motto: best service, most value
· Smart sales policy
A-ONE Alloy Service Items
· Non-standard product research and pre-production
· Fabrication of products
· Cutting, splitting for sheets and plates in stock
· Heat treatment(Solution treatment, aging harden treatment, anneal, spring temper, quench etc.)
· Surface finish(peeling, gridding)
· Logistics service
· Customized packing service(also for exporting)
· Import and export(A-ONE Alloy is certificated)
· Document translation
· Hard-to-find material sourcing
Customers of A-ONE Alloy
Customers of A-one Alloy are all over China (Taiwan and Hong Kong included). And we are exporting to USA, Canada, Italy, UK, Poland, Greece, Russia, Turkey, Iran, Israel, South Africa, South Korea, North Korea, India, Argentina, and Brazil and so on. Customers from 30+ countries trust us.
Where is A-ONE Alloy
A- A-ONE Alloy is located in No.2 Weihua Road, Suzhou Industrial Park, Jiangsu Province, China
B- ONE Alloy is around 130KM from Shanghai Pudong International Airport(PVG).
C- 13KM from Suzhou Railway Station
D- 7KM from Yangchenghu Station, Jinghu(G2) Highway
E- You can contact A-ONE Alloy sales for a pickup service